Thank you very much, and urgently seek the scientific maintenance method after floor pouring! We are a self-built frame concrete building, and the materials are stone powder, crushed stone and China R
Thank you very much, and urgently seek the scientific maintenance method after floor pouring! We are a self-built frame concrete building, and the materials are stone powder, crushed stone and China Resources 452 cement. Standard curing conditions of concrete: 20℃ 2℃, relative humidity above 95%, curing for 28d, which is a professional curing method.

Your temperature condition is reached, but the early strength of concrete will be affected if the relative humidity is above 95% and water is not soaked.

In the process of concrete setting and hardening, the hydration heat of cement is decreasing, so measures must be taken to cover it with straw mats, sacks and straw. And constantly sprinkling water, the best effect. First, these materials can avoid exposure to sunlight during the day, and second, they can absorb water. After sprinkling water, the water will evaporate after the cement releases heat, just to meet the humidity requirements.